Effect of Vinyl and Silicon Monomers on Mechanical and Degradation Properties of Bio-Degradable Jute-Biopol® Composite

dc.contributor.authorKhan, M. A.
dc.contributor.authorKopp, C.
dc.contributor.authorHinrichsen, G.
dc.date.accessioned2019-01-08T17:40:01Z
dc.date.available2019-01-08T17:40:01Z
dc.date.issued2001
dc.descriptionDieser Beitrag ist mit Zustimmung des Rechteinhabers aufgrund einer (DFG geförderten) Allianz- bzw. Nationallizenz frei zugänglich.de
dc.descriptionThis publication is with permission of the rights owner freely accessible due to an Alliance licence and a national licence (funded by the DFG, German Research Foundation) respectively.en
dc.description.abstractComposites of jute fabrics (Hessian cloth) and Biopol® were prepared by compression molding process. Three types of Biopol® (3-hydroxbutyrate-co-3-hydroxyvalarate) such as D300G, D400G and D600G, depending on the concentration of 3-hydroxyvalarate (3HV) in 3-hydroxbutyrate (3HB) were taken for this purpose. Mechanical properties such as tensile strength (TS), bending strength (BS), elongation at break (Eb) and impact strength (IS) of the jute-Biopol® composites were studied. It was found that the composite with D400G produced higher mechanical properties in comparison to the other two types of Biopol®. To increase mechanical properties as well as interfacial adhesion between fiber and matrix, 2-ethyl hydroxy acrylate (EHA), vinyl tri-methoxy silane (VMS) and 3-methacryloxypropyl tri-methoxy silane (MPS) were taken as coupling agents. Enhanced mechanical properties of the composites were obtained by using these coupling agents. Biopol® D400G composites showed the highest mechanical properties. Among the coupling agents EHA depicts the highest increase of mechanical properties such as tensile strength (80%), bending strength (81%), elongation at break (33%) and impact strength (130%) compared pure Biopol. SEM investigations demonstrate that the coupling agents improve the interfacial adhesion between fiber and matrix. The surface of the silanized jute was characterized by FTIR and found the deposition of silane on jute fiber was observed. Soil degradation test proved that the composite prepared with EHA treated jute exhibits better degradation properties in comparison to pure Biopol®.en
dc.identifier.eissn1530-7964
dc.identifier.issn0731-6844
dc.identifier.urihttps://depositonce.tu-berlin.de/handle/11303/8885
dc.identifier.urihttp://dx.doi.org/10.14279/depositonce-8014
dc.language.isoen
dc.rights.urihttp://rightsstatements.org/vocab/InC/1.0/
dc.subject.ddc660 Chemische Verfahrenstechnikde
dc.subject.othercompositeen
dc.subject.otherbiodegradableen
dc.subject.otherjuteen
dc.subject.othersilaneen
dc.subject.otherBiopol®en
dc.titleEffect of Vinyl and Silicon Monomers on Mechanical and Degradation Properties of Bio-Degradable Jute-Biopol® Compositeen
dc.typeArticleen
dc.type.versionpublishedVersionen
dcterms.bibliographicCitation.doi10.1106/RH67-0JVE-XX65-D39U
dcterms.bibliographicCitation.issue16
dcterms.bibliographicCitation.journaltitleJournal of Reinforced Plastics and Compositesen
dcterms.bibliographicCitation.originalpublishernameSAGE Publicationsen
dcterms.bibliographicCitation.originalpublisherplaceWashington, DCen
dcterms.bibliographicCitation.pageend1429
dcterms.bibliographicCitation.pagestart1414
dcterms.bibliographicCitation.volume20
tub.accessrights.dnbdomain
tub.affiliationFak. 3 Prozesswissenschaften::Inst. Werkstoffwissenschaften und -technologiende
tub.affiliation.facultyFak. 3 Prozesswissenschaftende
tub.affiliation.instituteInst. Werkstoffwissenschaften und -technologiende
tub.publisher.universityorinstitutionTechnische Universität Berlinde

Files

Original bundle
Now showing 1 - 1 of 1
Loading…
Thumbnail Image
Name:
Khan_et_al_2001.pdf
Size:
1.06 MB
Format:
Adobe Portable Document Format

Collections